Imikhiqizo

  • I-SUPER DUPLEX S32760 / F55 / 1.4501

    I-Super Duplex S32760/ F55 , I-Super Duplex Alloy UNS S32760 (F55 / 1.4501) inokumelana okuhle kakhulu kwe-Pitting ne-Crevice Corrosion emanzini olwandle emazingeni okushisa aphakeme, ehlinzekwa nge-PREN 40<(Pitting Resistance Eqv) .Ukumelana okuhle kakhulu ne-SCC (Stress Corrosion Cracking) endaweni eSour neChloride.

  • 17-7 Steel Strip, Coil, Foil, Wire, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043

    ● Iziphethu
    ● Amawasha
    ● Iziqeshana
    ●Izingxenye zokuhlinza
    ● Izinsimbi
    ● Izifutho
    ● Ikhekheba lezinyosi

  • Hastelloy B

    I-Hastelloy B iyisixazululo esiqinile esiqinisiwe, i-nickel-molybdenum alloy, enokumelana okuphawulekayo nokunciphisa izindawo ezifana negesi ye-hydrogen chloride, ne-sulfuric, acetic kanye ne-phosphoric acid.I-Molybdenum iyingxenye eyinhloko ye-alloying ehlinzeka ngokuphawulekayo ukumelana nokugqwala ekunciphiseni izindawo.Le ingxubevange yensimbi ye-nickel ingasetshenziswa esimweni esishiselwe ngenxa yokuthi imelana nokwakheka kwe-carbide ye-grain-boundary carbide endaweni ethinteke ekushiseni.

    Le nickel alloy inikeza ukumelana okuhle kakhulu ne-hydrochloric acid kukho konke ukugxila kanye namazinga okushisa.Ukwengeza, i-Hastelloy B2 inokumelana okuhle kakhulu nokugoba, ukuqhekeka kokugqwala kwengcindezi kanye nokuhlasela komugqa wommese kanye nokuhlaselwa kwendawo ethinteke ukushisa.Ingxubevange B inikeza ukumelana ne-sulfuric acid ehlanzekile kanye nenani lama-asidi angenayo i-oxidizing.

  • Haynes

    Ukushisa okuphezulu kwe-Alloy Chemery Chemical Ibanga C CO La nokunye akukho okudlula okungu-Haynes-188 0.2 0.5 ~ 0.5 1.25 ~ 0.515 ~ 23 2015 40 ~0.15 -
  • I-alloy 2205 Duplex Stainless Plate

    I-Sandmeyer Steel Company inohlu olubanzi lwe-2205 duplex stainless steel plate ngogqinsi ukusuka ku-3/16″ (4.8mm) ukuya ku-6″ (152.4mm).Amandla okukhiqiza cishe aphindwe kabili kunama-austenitic stainless steels, ngaleyo ndlela avumela umklami ukuthi onge isisindo futhi enze ingxubevange ibe nezindleko eziphakeme kakhulu uma iqhathaniswa no-316L noma 317L.

  • I-Incoloy

    I-High Temperature Alloy Chemical ukwakheka kweBanga C Si Mn SP Cr Ni Fe Al Ti Cu Mo okunye akukho okungaphezu kwe-Incoloy800 0.1 1 1.5 0.015 0.03 19~23 30~35 isisekelo 0.15~0.6 0.15~0.0001≤、0.601≤5≤5≤15~0.0001 ≞ 1 1.5 0.015 0.03 19~23 30~35 isisekelo 0.15~0.6 0.15~0.6 ≤0.75 — — I-Incoloy800HT 0.06~0.1 1 1.5 0.015 0.03~ 3~ isisekelo 3~ 313 0.15~0.6 ≤0.75 — Al+Ti 0.85...
  • SUPER DUPLEX 2507 Ikhwalithi ephezulu

    ● I-UNS S32750, F53
    ● ASTM A 240, A790, A815, A182, A 276, A 476, A789
    ● EN 1.4410
    ● Amanye amagama ajwayelekile SAF 2507®

  • I-Monel

    I-High Temperature Alloy Chemical ukwakheka kweBanga C Si Mn SP Cr Ni Mo Fe Co W Al Ti Cu akukho ngaphezu kwe-Monel400 0.3 0.5 2 0.024 - - isisekelo - ≤2.5 - - - - 28~34 Monel500 0.18 0.5 1.5 - 0≥3 -3 ≤2.5 - - - 28~34 Monel500 ≤2 - - 2.3~3.15 ​​0.35~0.85 27~33 Monel404 0.15 0.1 0.1 0.024 - - 52~57 - ≤0.5 ≤0.5 ≤0.5 - ≤0.5 ≤0.5
  • I-Austenite Stainless Steel

    I-High Temperature Alloy Chemical Ukwakheka kweBanga C Si Mn SP Cr Ni Mo Cu N okunye akukho okukhulu kuno-904L 0.02 1 2 0.015 0.03 19~21 24~26 4~5 1~2 - 253Ma 0.05~05~0 40 20.1 . ~22 10~12 - - 0.14~0.2 Ce0.03~0.08 254SMo 0.02 0.8 1 0.01 0.03 19.5~20.5 17.5~18.5 6~18.5 6~ 2-05 N 0.03 1 2 0.03 0.04 20–22 23.5~ 25.5 6–7 ≤0.75 0.18~...
  • Okubunjiwe, Okuyisicaba, Isikwele, Okuyindingilizi, Okuhle, Okuputshuliwe kanye Nocingo Olungenalutho ASTM A167, AMS 5523

    I-alloy 310S iyinsimbi engagqwali ye-chromium nickel ekwazi ukumelana ne-oxidation namandla emazingeni okushisa aphezulu kusevisi eqhubekayo efika ku-2000ºF (inqobo nje uma amagesi esibabule anciphisa abekho).Iphinde isetshenziselwe isevisi yezikhawu emazingeni okushisa afika ku-1900°F ngoba imelana nokuncishiswa futhi ine-coefficient ephansi yokunweba.Lesi sici sinciphisa ukuthambekela kwensimbi ukugoqa enkonzweni yokushisa.I-alloy 310S ifana ne-alloy 310 ngaphandle kokuqukethwe kwekhabhoni ephansi ukuze kuncishiswe imvula ye-carbide ngesikhathi sokushisela.

  • Imvula Eqinisa Insimbi Engagqwali

    I-High Temperature Alloy Chemical ukwakheka kweBanga C Si Mn SP Cr Ni Mo Cu Nb Al okunye akukho okukhulu kuno-0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~07-1070. 035 0.03 16–18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - 0.75b -1N00 14Cu 0.035 0.03 14–15.5 3.5~...
  • I-ALLOY 625 AMATERIAL DATA AMASHIDI

    Ingxubevange 625 iyingxubevange engeyona uzibuthe, ukugqwala – kanye ne-oxidation, esekelwe ku-nickel.Amandla ayo avelele nokuqina kwebanga lokushisa i-cryogenic kuya ku-2000°F (1093°C) asuselwe ikakhulukazi emiphumeleni yesixazululo esiqinile sezinsimbi eziphikisayo, i-columbium ne-molybdenum, ku-matrix ye-nickel-chromium.I-alloy inamandla amahle kakhulu wokukhathala kanye nokumelana nokucindezeleka-ukugqwala kokuqhekeka kuma-ion e-chloride.Ezinye izinhlelo zokusebenza ezijwayelekile ze-alloy 625 zihlanganisa izihlangu zokushisa, ihadiwe yesithando somlilo, ukudonsa kwenjini ye-turbine yegesi, amalayini omlilo nezinsimbi zokufutha, ihadiwe yezitshalo zamakhemikhali, kanye nezicelo ezikhethekile zamanzi olwandle.