  • I-HASTELLOY B2 UNS N10665 W.NR.2.4617

    I-Hastelloy B2 iyisixazululo esiqinile esiqinisiwe, i-nickel-molybdenum alloy, enokumelana okuphawulekayo nokunciphisa izindawo ezifana negesi ye-hydrogen chloride, ne-sulfuric, acetic kanye ne-phosphoric acid. I-Molybdenum iyingxenye eyinhloko ye-alloying ehlinzeka ngokuphawulekayo ukumelana nokugqwala ekunciphiseni izindawo. Le ingxubevange yensimbi ye-nickel ingasetshenziswa esimweni esishiselwe ngenxa yokuthi imelana nokwakheka kwe-carbide ye-grain-boundary carbide endaweni ethinteke ekushiseni.

    Le nickel alloy inikeza ukumelana okuhle kakhulu ne-hydrochloric acid kukho konke ukugxila kanye namazinga okushisa. Ukwengeza, i-Hastelloy B2 inokumelana okuhle kakhulu nokugoba, ukuqhekeka kokugqwala kwengcindezi kanye nokuhlasela komugqa wommese kanye nokuhlaselwa kwendawo ethinteke ukushisa. Ingxubevange B2 ihlinzeka ukumelana ne-sulfuric acid emsulwa kanye nenani lama-asidi angewona oxidizing.

  • I-Hastelloy

    Ukwakhiwa kwe-High Temperature Alloy Chemical Ibanga le-CPS Mn Si Ni Cr Co Cu Fe N Mo Al WV Ti enye ayikho ngaphezu kwe-HastelloyB 0.05 0.04 0.03 1 1 isisekelo ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - HastelloyB4 -2 0.02 0.04 0.03 1 0.1 isisekelo ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1~3 ≤3 ≤0.327 ≤0.5 ≤3 ≤0.2 ≤0.2 - ...
  • I-ALLOY 718 AMATERIAL DATA ishidi

    I-Inconel Alloy 718 Ingxubevange ye-nickel-chromium ekwazi ukujuluka ibe lukhuni futhi equkethe amanani abalulekile ensimbi, i-niobium, ne-molybdenum kanye namanani amancane e-aluminium ne-titanium. Ihlanganisa ukumelana nokugqwala namandla aphezulu nge-weldability evelele kuhlanganise nokumelana nokuqhekeka kwe-postweld. Ingxubevange inamandla amahle kakhulu okuqhekeka emazingeni okushisa ukuya ku-1300°F (700°C). Isetshenziswa kuma-turbines egesi, ama-rocket motors, imikhumbi-mkhathi, ama-reactors enuzi, amaphampu, namathuluzi. I-INCONEL alloy 718SPF™ iwuhlobo olukhethekile lwe-INCONEL alloy 718, eyenzelwe ukwakheka kweplasitiki.

    I-UNS: N07718

    I-W.Nr.: 2.4668

  • I-Monel 400 Uns N04400 W.Nr. 2.4360 Futhi 2.4361

    I-MONEL nickel-copper alloy 400 (UNS N04400) iyingxubevange enesixazululo esingaqiniswa kuphela ngokusebenza okubandayo. Inamandla aphezulu kanye nokuqina phezu kwezinga lokushisa elibanzi futhi imelana kahle kakhulu nezindawo eziningi ezonakalisayo. I-alloy 400 isetshenziswa kabanzi emikhakheni eminingi, ikakhulukazi ukucubungula olwandle namakhemikhali. Izicelo ezijwayelekile amavalvu namaphampu; i-pump kanye ne-propeller shafts; izinto zasolwandle nezinsimbi; izingxenye zikagesi neze-elekthronikhi; iziphethu; imishini yokucubungula amakhemikhali; amathangi kaphethiloli namanzi ahlanzekile; i-petroleum stills, imikhumbi yokucubungula kanye namapayipi; ama-heaters amanzi okuphakelayo kanye nezinye izishintshi zokushisa; nezishisi eziqeda amandla.Izakhi Zekhemikhali

  • I-Nimonic

    I-High Temperature Alloy Chemical ukwakheka kweBanga C Si Mn SP Cr Ni Fe Cu Ti Al Co okunye akukho okukhulu kune-Nimonic90 0.13 1 1 0.015 18~21 isisekelo ≤1.5 ≤0.2 2~3 1~2 15~21 ukuhola≤0 B≤0 ukuhola≤0 B≤0. ≤0.15 Nimonic91 0.1 1 1 0.015 27~30 isisekelo ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1 B0.002~0.01 IBanga Amandla ayishumi aphansi Zr≤0 IBanga Amandla ayishumi RmN/m㎡ Amandla Okukhiqiza Rp0.2N/...
  • I-ALLOY 825 AMATERIAL DATA ishidi

    I-Sandmeyer Steel Company stocks Alloy 825 nickel alloy plate ngogqinsi ukusuka .1875″ (4.8mm) ukuya ku-2.00″ (50.8mm) ukuze kusetshenziswe ukumelana nokugqwala ekulawuleni ukungcoliswa komoya, amakhemikhali kanye ne-petrochemical, ukucubungula ukudla, i-nuclear, uwoyela wasogwini nokukhiqizwa kwegesi , ukucubungula insimbi, ukucwengisiswa kwe-petroleum, ukucotshwa kwensimbi nokulahlwa kukadoti izimboni.

  • I-High Temperature Alloy

    I-Application Chemistry Typical Carbon 0.080 max Manganese 2.00 max Silicon 0.75 max Chromium 24.00- 26.00 Nickel 19.00- 22.00 Molybdenum 0.75 max Phosphorus 0.040 max 29 Physical Physical0. 9.01 g/cm³ I-Electrical Resistivity microhm-in (microhm-cm) 68°F (20°C) 37.0 (94.0) Ukushisa Okuthile BTU/lb/°F (kJ/kg•K) 32-212°F (0-100 °C) 0.12 (0.50) I-Thermal Conductivity BTU/hr/ft²/ft/°F (W/m•K) Ku-212°F (100°C) 8....
  • I-Nitronic

    I-High Temperature Alloy Chemical Ukwakheka kweBanga C Si Mn SP Cr Ni Fe Mo Ti Cu Nb N okunye akukho okukhulu kune-Nitronic50 0.06 1 4~6 0.03 0.04 20.5~23.5 11.5~13.5 isisekelo 1.5~3 >3 > 3 .> . 0.2~0.4 - Nitronic60 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 base — — — — 0.08~0.18 - Alloy property minimum Grade state tensile strength RmN/mp0 St. Njengo% B...
  • 17-4PH Ishidi Ledatha Yezinto Ezibalulekile

    Izihlonzi zamazwe ngamazwe

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • I-High Precision Alloy

    Ukwakheka kwe-High Temperature Alloy Chemical Ibanga C Si Mn SP Cr Ni Mo Cu Fe Al Co Ti akukho ngaphezu kuka-1J50 0.03 0.15~0.3 0.3~0.6 0.02 0.02 - 49.5~50.5 - ≤0.1J isisekelo .~ 0.2 0.3 0.3 0.3 0.3 0.3 7 . 0.6~1.1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 isisekelo — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2~5.8 440.5~ 5.8 440.5 isisekelo. 0.5–0.8 — 2.3–2.7 4J29 0.03 0.3 0.5 0.02 0.02 ...
  • I-Nickel

    Ukwakheka kwe-High Temperature Alloy Chemical Ibanga le-Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.4 ≤0.0. ≤0.01 ≤0.35 I-alloy property ubuncane besimo somkhiqizo wesimo sokuqina kwamandla RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% Brinell hardness HB stick and strip hot rolled 60~85 15~45 35~55 4 induku ukukhishwa amakhaza noma ukuncibilika 55-75 15...
  • I-Biphase Stainless Steel

    I-High Temperature Alloy Chemical Ukwakheka kweBanga C Si Mn SP Cr Ni Mo Cu NW okunye okungaphezu kuka-F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - 002 .002 .002 . 329 0.08 1 1.5 0.03 0.035 23~28 3~6 1~3 - - - - A4 ...