◆ I-Haynes-188 inamandla okushisa aphezulu, izakhiwo ezinhle ze-anti-oxidation kanye ne-anti-corrosion, esetshenziswa kabanzi ku-aerospace, i-petrochemical, ukwakha umkhumbi neminye imikhakha.

Ukwakheka kwamakhemikhali

Ibanga

C

Si

Mn

S

P

Cr

Ni

Fe

B

Co

W

La

okunye

akukho okukhulu kune

Haynes-188

0.05-0.15

0.2-0.5

1.25

0.015

0.02

21-23

20 - 24

≤3

≤0.015

40; 45

13-15

0.03-0.15

-