    I-Hastelloy B iyisixazululo esiqinile esiqinisiwe, i-nickel-molybdenum alloy, enokumelana okuphawulekayo nokunciphisa izindawo ezifana negesi ye-hydrogen chloride, ne-sulfuric, acetic kanye ne-phosphoric acid. I-Molybdenum iyingxenye eyinhloko ye-alloying ehlinzeka ngokuphawulekayo ukumelana nokugqwala ekunciphiseni izindawo. Le ingxubevange yensimbi ye-nickel ingasetshenziswa esimweni esishiselwe ngenxa yokuthi imelana nokwakheka kwe-carbide ye-grain-boundary carbide endaweni ethinteke ekushiseni.

    Le nickel alloy inikeza ukumelana okuhle kakhulu ne-hydrochloric acid kukho konke ukugxila kanye namazinga okushisa. Ukwengeza, i-Hastelloy B2 inokumelana okuhle kakhulu nokugoba, ukuqhekeka kokugqwala kwengcindezi kanye nokuhlasela komugqa wommese kanye nokuhlaselwa kwendawo ethinteke ukushisa. Ingxubevange B inikeza ukumelana ne-sulfuric acid ehlanzekile kanye nenani lama-asidi angenayo i-oxidizing.

  • I-HASTELLOY B2 UNS N10665 W.NR.2.4617

    I-Hastelloy B2 iyisixazululo esiqinile esiqinisiwe, i-nickel-molybdenum alloy, enokumelana okuphawulekayo nokunciphisa izindawo ezifana negesi ye-hydrogen chloride, ne-sulfuric, acetic kanye ne-phosphoric acid. I-Molybdenum iyingxenye eyinhloko ye-alloying ehlinzeka ngokuphawulekayo ukumelana nokugqwala ekunciphiseni izindawo. Le ingxubevange yensimbi ye-nickel ingasetshenziswa esimweni esishiselwe ngenxa yokuthi imelana nokwakheka kwe-carbide ye-grain-boundary carbide endaweni ethinteke ekushiseni.

    Le nickel alloy inikeza ukumelana okuhle kakhulu ne-hydrochloric acid kukho konke ukugxila kanye namazinga okushisa. Ukwengeza, i-Hastelloy B2 inokumelana okuhle kakhulu nokugoba, ukuqhekeka kokugqwala kwengcindezi kanye nokuhlasela komugqa wommese kanye nokuhlaselwa kwendawo ethinteke ukushisa. Ingxubevange B2 ihlinzeka ukumelana ne-sulfuric acid emsulwa kanye nenani lama-asidi angewona oxidizing.

  • I-Hastelloy

    Ukwakhiwa kwe-High Temperature Alloy Chemical Ibanga le-CPS Mn Si Ni Cr Co Cu Fe N Mo Al WV Ti enye ayikho ngaphezu kwe-HastelloyB 0.05 0.04 0.03 1 1 isisekelo ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - HastelloyB4 -2 0.02 0.04 0.03 1 0.1 isisekelo ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1.32 ≥65 1.32 ≥65 1 32 ≤0.5 ≤ 3 ≤0.2 ≤0.2 - ...
  • I-Hastelloy C-276 AMASHIDI EDATHA YEMPAHLA

    I-HASTELLOY C276, i-UNS N10276 ithathwa njengengxube ye-nickel ekwazi ukumelana nokugqwala etholakala ngezindlela eziningi. Ingxubevange C-276 futhi inokumelana okuhle kakhulu nomgodi, ukuqhekeka kwe-stress-corrosion, kulungele ikakhulukazi ukusetshenziswa ekushiseni okuphezulu, ama-asidi angaphilayo kanye nama-organic acid axutshwe nokungcola (okufana ne-formic acid ne-acetic acid), kanye nezindawo ezigqwala emanzini olwandle.

  • I-alloy 2205 Duplex Stainless Plate

    I-Sandmeyer Steel Company inohlu olubanzi lwe-2205 duplex stainless steel plate ngogqinsi ukusuka ku-3/16″ (4.8mm) ukuya ku-6″ (152.4mm). Amandla okukhiqiza cishe aphindwe kabili kunama-austenitic stainless steels, ngaleyo ndlela avumela umklami ukuthi onge isisindo futhi enze ingxubevange ibe nezindleko eziphakeme kakhulu uma iqhathaniswa no-316L noma 317L.