Thayipha i-17-7PH® Precipitation Hardening Alloy iyinsimbi engagqwali elingana ne-austenitic ene-austenitic esimweni esine-anneal, kodwa i-martensitic esimweni esiqinile. Uhlobo lwe-17-7PH® lunikeza amandla aphezulu nobulukhuni, izici ezinhle kakhulu zokukhathala, ukumelana nokugqwala okuhle kanye nokuhlanekezela okuncane ekwelapheni ukushisa. Yakheka kalula esimweni esine-anneal, bese iqiniswa kumazinga aphezulu amandla ngokwelashwa okulula kokushisa kuZimo RH 950 kanye ne-TH 1050. Amandla aphezulu kakhulu e-Condition CH 900 anikeza izinzuzo eziningi lapho i-ductility elinganiselwe nokusebenza kuvunyelwe. Esimeni sayo sokwelashwa ngokushisa, le ngxubevange ihlinzeka ngezakhiwo ezihlukile zomshini emazingeni okushisa afika ku-900 °F (482 °C).

I-N08367 - 1.4529 - I-Incoloy 926 imigoqo

CHEMISTRY TYPICAL

Inconel 825 imigoqo

Ikhabhoni: 0.090 ubuningi

I-Manganese: 1.00 max

I-silicon: 1.00 max

I-Chromium: 16.00-18.00

I-Nickel: 6.50- 7.75

I-aluminium: 0.75-1.50

I-Phosphorus: 0.040 max

Isibabule: 0.030 ubuningi

Insimbi: Ibhalansi

IZIMPAHLA ZOMZIMBA

Ukuminyana: (I-Cond. A): 0.282 lbs/in3 7.80 g/cm3

Ukungazweli Ugesi: (microhm-cm) (zonke izimo): 60 °F (20 °C): 80

I-Thermal Conductivity: BTU/hr/ft2/ft/°F (W/m•K)

Ku-300 °F (149 °C): 9.5 (16.5)

I-Mean Coefficient of Thermal Expansion: in/inl°F (µm/m•K): (Cond. A):

70 -200 °F (21 -93 °C): 8.5 x 10-5 (15.3)

70 -400 °F (21 -204 °C): 9.0 x 10-5 (16.2)

70 -600 °F (21 -315 °C): 9.5 x 10-5 (17.1)

70 -800 °F (21 -427 °C): 9.6 x 1 o-6 (16.0)

I-Modulus of Elasticity: ksi (MPa)

29 x 103 (200 x 103) ku-tension

I-Magnetic Permeability:

I-Annealed: I-ferromagnetic ebuthakathaka

Ukwelashwa kokushisa: I-ferromagnetic enamandla

AMAFOMU

I-Strip Coil

  • I-17-7PH I-Stainless Steel Strip
  • 17-7PH Icwecwe Lensimbi Engagqwali
  • 17-7PH Iribhoni Lensimbi Engagqwali

Imikhiqizo Yocingo

  • 17-7PH I-Stainless Steel Shaped Wire & Nocingo Lwephrofayela
  • 17-7PH Insimbi Engagqwali Eyindilinga
  • 17-7PH Intambo Yensimbi Engenasici
  • 17-7PH I-Stainless Steel Square Wire
Inconel 825 imigoqo
Inconel 600 amapuleti aginqiwe ashisayo

Ukusebenza

Icubungula Izakhiwo Zemishini Emazingeni Okushisa Egumbi

Ibanga Lokulinganisa:<.010 amayintshi

Amandla Okuqina Okuqinile: 150 KSI max (1035 MPa max)

Amandla Okukhiqiza (0.2% offset): 65 KSI max (450 MPa max)

Ukwelulwa: Xhumana ne-Ulbrich Technical Services

Ibanga Lokulinganisa: > .010 amayintshi

Amandla Okuqina Okuqinile: 150 KSI max (1035 MPa max)

Amandla Okukhiqiza (0.2% offset): 55 KSI max (380 MPa max)

Ubude: 20% min

Ukuqina: Rb 92 max

Isimo Esijwayelekile C

Amandla Okuqina Okuqinile: 200 KSI min (1380 MPa min)

Amandla Esivuno (0.2% offset): 175 KSI min (1205 MPa min)

Ubude: 1 % min

Ukuqina: Re 41 min (inhloso)

EZENGEZIWE AMA TEMPERS aginqiwe:

Xhumana ne-Ulbrich Technical Services uma kudingeka ulaka ngaphandle kweSimo C.

UKWELASHWA KOKUSHISA KWE-17-7PH Stainless Steel

I-TH 1050 Ejwayelekile

Amandla Okuqina Okuqinile: 180 KSI min (1240 MPa min)

Amandla Esivuno: (0.2% Offset) 150 KSI min (1034 MPa min)

Ukwelulwa: Xhumana ne-Ulbrich Technical Services

Ukuqina: Re 38 min

I-RH950 ejwayelekile

Amandla Okuqina Okuqinile: 210 KSI min (1450 MPa min)

Amandla Esivuno: (0.2 Offset) 190 KSI min (1310 MPa min)

Ukwelulwa: Xhumana ne-Ulbrich Technical Services

Ukuqina: Re 44 min

I-CH900 Ejwayelekile

Amandla Okuqina Okuqinile: 240 KSI min (1655 MPa min)

Amandla Esivuno: (0.2% Offset) 230 KSI min (1586 MPa min)

Ubude: 1 % min

Ukuqina: Re 46 min (inhloso)

IZIMPAHLA EZENGEZIWE

UKUMELANA KOKUGULA KOKUNGU-17-7PH ENGAGWAZI

Bheka ku-NACE (National Association of Corrosion Engineers) ukuze uthole izincomo.